Polyurethane elastomer common problems and solutions


Release time:

2024-06-19

1. need to reduce the viscosity of prepolymer

 

(1) Optimum synthesis temperature of prepolymer;

(2) Add polyols to isocyanate;

(3) Increase mixing;

(4) Control the reaction speed to a slower degree;

(5) Use the right catalyst;

(6) Strictly control the moisture content of raw materials, and the moisture content should be less than 0.05%;

(7) The preparation of prepolymers should be carried out under acidic conditions.

 

2. Yellowing problem

 

(1) Add antioxidant or UV stabilizer;

(2) Use aliphatic isocyanates.

 

3. NCO is lower than the theoretical value

 

(1) Water enters the reaction system;

(2) the proportion is not correct;

(3) isocyanate loss;

(4) Side reactions caused by alkalinity

 

4. NCO is higher than the theoretical value

 

(1) The reaction time is too short;

(2) the amount of catalyst is insufficient or the catalyst is inappropriate;

(3) the reaction temperature is too low;

(4) The ratio is wrong

 

5. Causes of bubbles

 

(1) Water enters the reaction system;

(2) degassing is incomplete;

(3) mixing is not suitable;

(4) Bubbles are involved during pouring

 

6. How to dry the main raw materials

 

(1) The polyol is dried in high temperature, vacuum, stirring, vibrating [wiki] equipment [/wiki];

(2) Drum drying nitrogen drying

 

7. Reaction speed is too fast

 

(1) The alkaline is too high;

(2) too much catalytic dose;

(3) Raising the temperature too fast (for every 10 degrees Celsius increase, the life of the kettle is shortened by 2 times)

 

8, the reaction speed is too slow

 

(1) Insufficient catalytic dose;

(2) The reaction temperature is too low

 

9, improve wear resistance

 

(1) The use of appropriate primary raw materials, especially hard segment materials;

(2) Use Teflon additives

 

10, improve low temperature flexibility

 

(1) Use polyether polyols with higher molecular weight instead of polyether polyols;

(2) Use PTMEG instead of PPG

 

11, improve high temperature resistance

 

(1) The use of high-performance raw material ingredients, especially chain extenders and isocyanates (such as HQEE, PPDI);

(2) Use the most stable antioxidant

 

12, how to improve compression permanent change

 

(1) The use of appropriate primary raw materials;

(2) The use of three-functional chain extender;

(3) Adopt a higher NCO index;

(4) Optimize the mixing temperature;

(5) Use three-functional isocyanate

 

13. How to reduce energy absorption

 

Use materials that have linear polymerization, do not form branch chains and form good hard segment properties

 

14, how to make transparent PU

 

(1) Reduce the crystallinity of the hard segment (suitable processing conditions and/or with special chain extenders);

(2) Change NCO%;

(3) The order degree of the hard segment is disrupted